I-6J13/I-6J8/I-6J12I-Copper-Maninganese-Nickel Alloy yeIManigan Shunt
I-alloy yokumelana ne-alloy ye-aloy ibonakala ngokukhethekile ngokulinganisa okushisa okuphansi phakathi kuka-20 no-50 ° C
Kodwa-ke, imithwalo ephakeme eshisayo esezingeni elingelona ox-oxidizing kungenzeka. Lapho isetshenziselwa ukumelana ngokunemba ngezidingo eziphakeme kakhulu, abamelana nalokhu kufanele bazinze ngokucophelela futhi izinga lokushisa lesicelo akufanele lidlule ku-60 ° C. Ukudlula izinga lokushisa eliphakeme emoyeni kungahle kuholele ekunciphisweni kwe-Drift okwenziwe ngezinqubo ze-oxidizing.thus, ukuqina kwesikhathi eside kungathinteka kabi. Ngenxa yalokhu, ukumelana kanye nokulinganisa okushisa kokumelana nogesi kungashintsha kancane. Iphinde isetshenziswe njengezinto eziphansi zezindleko zokubuyiselwa kwezindleko zesiliva esiliva ukukhwela i-hard metal.
Ukucacisa
I-Mangagan Wire / Cound12NI2 Wire esetshenziswerheostats, ukumelana, shunt etc mangagan wire 0.08mm kuya ku-10mm 6j13, 6J12, 6J11 6J8
I-Mangagan Wire (CUPRO-MANGANESE Foure) yigama elinethezekile le-alloy ye-86% yethusi yethusi, i-12% manganese, kanye no-2-5% nickel.
I-Mangagan Wire kanye ne-Foil isetshenziswa emkhathweni we-Resistor, ikakhulukazi ama-ammeter shunts, ngenxa yokushisa kwayo kwe-zero yerombo
Ukusetshenziswa Manganin
I-Manigan Foil ne-Wire isetshenziswa ekwenziweni kwe-Resistor, ikakhulukazi i-Ammeter Shunt, ngenxa ye-coeffient yayo yokushisa ye-zero cishe yenani lokumelana nokuqina kwesikhathi eside.
I-ALLOOY evuthayo ephansi ye-Copper ephansi isetshenziswa kabanzi ekwephule kakhulu kwe-voltage voltage breaker, i-thermal ngokweqile edluliselwe phambili, kanye neminye umkhiqizo kagesi ophansi. Ingenye yezinto ezibalulekile zemikhiqizo kagesi ephansi ye-voltage. Izinto ezikhiqizwa yinkampani yethu zinezici zokungalingani kahle okuhle nokuqina okuphezulu. Singanikeza zonke izinhlobo zezintambo eziyindilinga, izimbotshana nezinto zokuphepha.