Ngenxa yokugcwala okuphezulu kokufakwa kukazibuthe, lapho kwenziwa injini yamandla alinganayo, inganciphisa kakhulu ivolumu, lapho yenza i-electromagnetic, ngaphansi kwendawo efanayo ye-cross-sectional, ingakhiqiza amandla amakhulu okudonsa.
Ngenxa yephoyinti layo eliphakeme le-Curie, ingxubevange ingasetshenziswa kwezinye izinto ezithambile zikamagnetic alloy ezisuswe uzibuthe ngokuphelele ngaphansi kwezinga lokushisa eliphezulu, futhi zigcine ukuzinza okuhle kazibuthe.
Ngenxa ye-coefficient enkulu ye-magnetostrictive, futhi ifanele ukusetshenziswa njenge-transducer yamagnetostrictive, amandla okukhiphayo aphezulu, ukusebenza kahle kuphezulu. I-resistivity ye-alloy ephansi (0.27 μΩ m.), ayifanele ukusetshenziswa ngaphansi kwefrikhwensi ephezulu. Intengo iphakeme, i-oxidized kalula, futhi ukusebenza kokucubungula kubi; ukwengeza i-nickel efanelekile noma ezinye izakhi kungathuthukisa ukusebenza kokucubungula.
Isicelo: kufanelekile ukwenza ikhwalithi ilula, ivolumu encane yendiza kanye nendiza yasemkhathini enezingxenye zikagesi, njengokuthi, i-micro-motor rotor magnet pole head, ama-relay, ama-transducer, njll.
Okuqukethwe Kwekhemikhali(%)
Mn | Ni | V | C | Si | P | S | Fe | Co |
0.30 | 0.50 | 0.8-1.80 | 0.04 | 0.30 | 0.020 | 0.020 | U-Bal | 49.0-51.0 |
Izakhiwo Zemishini
Ukuminyana | 8.2 g/cm3 |
I-Thermal Expansion Coefficient (20~100ºC) | 8.5 x 10-6 /ºC |
I-Curie Point | 980ºC |
Ukungazweli Kwevolumu (20ºC) | 40 μΩ.cm |
I-Saturation Magnetic Stricture Coefficient | 60 x 10-6 |
Amandla Okuphoqa | 128A/m |
Amandla wokungeniswa kazibuthe endaweni ehlukene kazibuthe
B400 | 1.6 |
B800 | 1.8 |
B1600 | 2.0 |
B2400 | 2.1 |
B4000 | 2.15 |
B8000 | 2.35 |