Izintambo ze-Nickel-Chrome zisetshenziswa kabanzi njenge-alloy yokumelana okuphezulu kokushisa kukagesi kanye nama-resistors enxeba lensimbi embonini yensimbi, embonini yamakhemikhali kanye nasembonini kagesi, njll.
Le ntambo ye-alloy ine-coefficient ephezulu yokumelana nogesi, i-anti-oxidation enhle kanye nokusebenza kahle kokulwa nokugqwala, futhi inamandla okusebenza kahle kwemishini kanye nokushibilika, enamandla aphezulu ekushiseni okuphezulu.
Izici eziyinhloko zama-alloy okushisa kagesi e-Ni-Cr kanye ne-Ni-Cr-Fe
| Uhlobo | I-Cr30Ni70 | I-Cr15Ni60 | I-Cr20Ni35 | I-Cr20Ni80 | I-Cr20Ni30 | I-Cr25Ni20 | |
| Ukusebenza | |||||||
| Ukwakheka Okuyinhloko Kwamakhemikhali | Ni | Ukuphumula | 55.0-61.0 | 34.0-37.0 | Ukuphumula | 30.0-30.4 | 19.0-22.0 |
| Cr | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 20.0-23.0 | 18.0-21.0 | 24.0-26.0 | |
| Fe | ≤ 1.0 | Ukuphumula | Ukuphumula | ≤ 1.0 | Ukuphumula | Ukuphumula | |
| Izinga lokushisa eliphezulu lesevisi eqhubekayo yento | 1250 | 1150 | 1100 | 1200 | 1100 | 1050 | |
| Ukumelana nokushisa ku-20ºC (μΩ m) | 1.18±0.05 | 1.12±0.05 | 1.04±0.05 | 1.09±0.05 | 1.06±0.05 | 0.95±0.05 | |
| Ubuningi (g/cm³) | 8.10 | 8.20 | 7.90 | 8.40 | 7.90 | 7.15 | |
| Ukuqhuba kwe-thermal (KJ/mh ºC) | 45.2 | 45.2 | 43.5 | 60.3 | 43.8 | 43.8 | |
| Ukwandiswa kwe-Coefficient yemigqa (αx10-6/ºC) | 17.0 | 17.0 | 19.0 | 18.0 | 19.0 | 19.0 | |
| Indawo yokuncibilika (cishe) (ºC) | 1380 | 1390 | 1390 | 1400 | 1390 | 1400 | |
| Ukwelulwa ekuqhekekeni (%) | > 20 | > 20 | > 20 | > 20 | > 20 | > 20 | |
| Isakhiwo se-Micrographic | i-austenite | i-austenite | i-austenite | i-austenite | i-austenite | i-austenite | |
| Izakhiwo zikamazibuthe | okungeyona i-magnetic | Amandla kazibuthe aphansi | Amandla kazibuthe aphansi | okungeyona i-magnetic | Amandla kazibuthe aphansi | okungeyona i-magnetic | |