I-SWG16 0Cr21Al4 / 0Cr19Al3 I-fecral alloy Heating Wire yokudwetshwa kabusha
I-Resistance Wire eyenziwe Nge-Nickel Chrome Alloys, Nickel Chrome Iron Alloys, Iron Chrome Aluminium Alloys, Copper Nickel Alloys.
Isetshenziswa kakhulu ku-heater, isici sokushisa kanye ne-resistor, njll.
NiCr 80/20, NiCr 70/30, NiCr 60/15, NiCr 35/20
CrAl 15-5, CrAl 20-5, CrAl 25-5, njll...
Constantan, Alloy 30, Alloy 60, Alloy 90, njll.
Ukumelana Nogesi kusuka ku-0.02 u ohm/m-1.53 u ohm/m
Izinga Lokushisa Lokusebenza kusuka ku-200 C kuya ku-1400 C
Pls khululeka ukuxhumana nathi uma kukhona umbuzo.
I-NiCr:
RESISTOHM 20, RESISTOHM 30, RESISTOHM 40, RESISTOHM 60, RESISTOHM 70, RESISTOHM 80
I-FeCrAl:
I-RESISTOHM 125, RESISTOHM 135, RESISTOHM 140,
I-RESISTOHM 145, RESISTOHM 153
Kunini
Constantan, Cuprothal 5, Cuprothal 10, Cuprothal 15, Cuprothal 30, Eurica
Ibanga le-FeCrAl Alloy | Ukwakheka Kwekhemikhali % | |||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | Re | Abanye |
ubuningi(≤) | ||||||||||
1Cr13Al4 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 12.5-15.0 | —- | 3.5-4.5 | 0.1 | U-Bal. |
0Cr15Al5 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 14.5-15.5 | —- | 4.5-5.3 | 0.1 | U-Bal. |
0Cr25Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 23.0-26.0 | ≤0.60 | 4.5-6.5 | 0.1 | U-Bal. |
0Cr23Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 20.5-23.5 | ≤0.60 | 4.2-5.3 | 0.1 | U-Bal. |
0Cr21Al6 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 19.0-22.0 | ≤0.60 | 5.0-7.0 | 0.1 | U-Bal. |
0Cr21Al4 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 21.0-23.0 | ≤0.60 | 3.0-5.2 | 0.1 | U-Bal. |
0Cr21Al6Nb | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.60 | 21.0-23.0 | ≤0.60 | 5.0-7.0 | 0.1 | U-Bal. |
0Cr27Al7Mo2 | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.40 | 26.5-27.8 | ≤0.60 | 6.0-7.0 | 0.1 | U-Bal. |
Ukubunjwa Kwamakhemikhali Nezakhiwo:
Izakhiwo/Ibanga | I-NiCr 80/20 | I-NiCr 70/30 | I-NiCr 60/15 | I-NiCr 35/20 | I-NiCr 30/20 | |
Ukwakhiwa Kwekhemikhali Eyinhloko(%) | Ni | U-Bal. | U-Bal. | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1.0 | ≤ 1.0 | U-Bal. | U-Bal. | U-Bal. | |
Izinga Lokushisa Elisebenzayo Eliphezulu(ºC) | 1200 | 1250 | 1150 | 1100 | 1100 | |
Ukumelana no-20ºC (μ Ω · m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
Ukuminyana(g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
I-Thermal Conductivity (KJ/m· h· ºC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
I-Coefficient of Thermal Expansion(α × 10-6/ºC) | 18 | 17 | 17 | 19 | 19 | |
I-Melting Point(ºC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Ubude(%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Isakhiwo seMicrographic | i-austenite | i-austenite | i-austenite | i-austenite | i-austenite | |
Impahla Magnetic | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic | nonmagnetic |
I-CuNi Alloys Grade | Ukumelana nogesi (20degreeΩ mm²/m) | I-coefficient yokushisa yokumelana (10^6/degree) | Ukuminyana g/mm² | Ubukhulu. izinga lokushisa (iziqu) | Iphoyinti lokuncibilika (iziqu) |
KuNi1 | 0.03 | < 1000 | 8.9 | 200 | 1085 |
KuNi2 | 0.05 | < 1200 | 8.9 | 200 | 1090 |
Kuni6 | 0.10 | < 600 | 8.9 | 220 | 1095 |
Kunini8 | 0.12 | < 570 | 8.9 | 250 | 1097 |
KuNi10 | 0.15 | < 500 | 8.9 | 250 | 1100 |
CuNi14 | 0.20 | <380 | 8.9 | 300 | 1115 |
Kunini19 | 0.25 | < 250 | 8.9 | 300 | 1135 |
Kunini22 | 0.30 | < 160 | 8.9 | 300 | 1150 |
KuNi30 | 0.35 | < 100 | 8.9 | 350 | 1170 |
CuNi34 | 0.40 | -0 | 8.9 | 350 | 1180 |
CuNi40 | 0.48 | ± 40 | 8.9 | 400 | 1280 |
ICuNi44 | 0.50 | <-6 | 8.9 | 400 | 1280 |