I-Spiralizinto zokushisa zikagesiyakhiwe ngemijikelezo eyindilinga eyakhiwe yintambo eyodwa noma ezimbili ezimelana ne-alloy efanelekile kuye ngokuthi isetshenziswa kanjani.
Izici zayo eziyinhloko zifaka phakathi ukufakwa kwento yokushisa yensimbi ye-nickel-chrome alloy kanye nokucindezeleka okujwayelekile okungu--230 V.
Izicelo ezivamile yilezi: imishini yokomisa yezimboni, ama-air heater, izitofu, njll.
Ngaphezu kwalokho, futhi ngokusho kwentambo ye-alloy eziqukethe, singahlukanisa izinhlobo ezintathu zamamodeli:
| C | P | S | Mn | Si | Cr | Ni | Al | Fe | Okunye |
| Ubuningi | |||||||||
| 0.03 | 0.02 | 0.015 | 0.60 | 0.75~1.60 | 20.0~23.0 | Ibhalansi. | Umkhawulo ongu-0.50 | Ubuningi obungu-1.0 | - |
Izakhiwo Zemishini Zentambo Ye-nichrome
| Izinga Lokushisa Eliphezulu Lesevisi Eqhubekayo: | 1200ºC |
| Ukuqina kokushisa okungu-20ºC: | 1.09 ohm mm2/m |
| Ubuningi: | 8.4 g/cm3 |
| Ukuqhuba Ukushisa: | 60.3 KJ/m·h·ºC |
| Isilinganiso Sokwanda Kokushisa: | 18 α×10-6/ºC |
| Indawo Yokuncibilika: | 1400ºC |
| Ukwelulwa: | Ubuncane obungu-20% |
| Isakhiwo se-Micrographic: | I-Austenite |
| Impahla Kamagnetic: | okungeyona i-magnetic |
Izici Zokushisa Zokumelana Nogesi
| 20ºC | 100ºC | 200ºC | 300ºC | 400ºC | 500ºC | 600ºC |
| 1 | 1.006 | 1.012 | 1.018 | 1.025 | 1.026 | 1.018 |
| 700ºC | 800ºC | 900ºC | 1000ºC | 1100ºC | 1200ºC | 1300ºC |
| 1.01 | 1.008 | 1.01 | 1.014 | 1.021 | 1.025 | - |
Usayizi ojwayelekile wentambo ye-Nickel alloy:
Sihlinzeka ngemikhiqizo esesimweni sentambo, ucingo oluyisicaba, umcu. Singenza nezinto ezenziwe ngokwezifiso ngokwezicelo zabasebenzisi.
Intambo ekhanyayo nemhlophe–0.025mm~3mm
Ucingo lokukha: 1.8mm ~ 10mm
Intambo ehlanganisiwe: 0.6mm ~ 10mm
Ucingo oluyisicaba: ukujiya 0.05mm ~ 1.0mm, ububanzi 0.5mm ~ 5.0mm


150 0000 2421